Why PEI Dosage Drifts: Amine Value, Solids and Viscosity (CAS 9002-98-6)

Nov 17, 2026

Dosing & Analytical Guide

How The Amine Value, Solids And Viscosity On A PEI Certificate Convert Into A Dose - And Why Two Drums Of One Grade Behave Differently

A polyethyleneimine (CAS 9002-98-6) trial looks simple until two drums of the same grade behave differently. The number that governs performance is not the grade name but the amine value on the certificate.

Origin: Zhengzhou, China  |  Author: Technical Team, Alfa Chemical
⚡ The Core Insight
If your Polyethyleneimine (PEI, CAS 9002-98-6) dose works in a jar test and underperforms in the plant, the grade is rarely the problem. The amine value you dosed against is. A 50% aqueous grade carries half the amine value per gram of the neat polymer, and a drum that has absorbed moisture carries less again. Dosing from the catalogue grade name instead of the lot certificate is the single most common reason two trials at the same dose give different results.

1. What the PEI Amine Value Actually Counts

Branched polyethyleneimine carries primary, secondary and tertiary amines on the same chain, in roughly a one-to-two-to-one ratio. All three are basic, so a potentiometric titration with standard acid counts total basic nitrogen rather than one specific group. The result is therefore reported as a single figure, and two suppliers using different endpoints can publish numbers that are not directly comparable.

The unit is normally mmol/g. Some certificates use mg KOH/g. The conversion is fixed - multiply by 56.1 - so 19 mmol/g equals about 1,066 mg KOH/g. Confirm which unit a certificate uses before setting it against your own historical data.

2. PEI at 50% Solids: Why the Same Grade Reads Differently

This is where most dosing errors start. A certificate issued on a dry basis describes the polymer; a certificate issued as supplied describes the drum. For a 50% aqueous grade the two differ by a factor of two before any batch variation is considered. A buyer comparing two suppliers, one quoting dry and one as supplied, will conclude that one material is twice as reactive when nothing has changed.

The practical rule: normalise every figure to dry basis before comparing anything, and state both figures in your own specification, together with a loss on drying tolerance. Alfa Chemical supplies PEI grades with loss on drying controlled to 5.0% or below, and reports the measured value for each lot.

3. Converting the PEI Amine Value Into a Starting Dose

For charge neutralisation and flocculant dosing - clay suspension, pigment dispersion, wet-end addition - the useful quantity is milliequivalents per gram, which is numerically equal to the amine value in mmol/g. Divide the anionic demand of the system by that figure and you have a stoichiometric starting point for the jar test.

Parameter
Typical Handling
Amine value basis
Dry basis for comparison, as supplied for dosing
Worked example
19 mmol/g dry, 50% solution = 9.5 mmol/g supplied
Demand of 0.6 mmol/L
0.6 / 9.5 = 63 mg/L as the centre point
What that number is not
A setpoint; bracket it either side in the bench series

Figures above are illustrative. Use the amine value for the lot you receive, and confirm the final dose on your own system.

Two corrections matter more than the arithmetic. Only a fraction of the amines are protonated at the working pH, so the effective charge at pH 7 sits well below the total amine value. And in high-solids or high-shear systems polymer is consumed on surfaces other than the target particles. Both push the practical dose above the stoichiometric figure. The same calculation applies to every polyethyleneimine grade, CAS 9002-98-6, from 600 to 70,000.

4. PEI Viscosity and Pumpability

Across the PEI range viscosity runs from roughly 200 to 150,000 mPa·s at 25 °C, depending on grade and solids. A viscosity figure without solids content and temperature cannot be compared to anything, because dilution changes it by orders of magnitude rather than by percentages. A line sized on the neat polymer may not handle the 50% solution, and the reverse also happens.

Two operating points avoid most transfer problems: keep the solution above 10 °C so it does not gel in the line, and dose into the dilute side of the process where mixing energy is available. Adding neat polymer into a high-solids stream is the usual cause of gel slugs and blocked injection quills.

5. Why a Stored PEI Drum Titrates Lower

Three mechanisms explain most of the gap between a release certificate and a re-test six months later. PEI is hygroscopic, so a drum that has taken up moisture shows less amine value per gram because more of that gram is water. Primary amines react with atmospheric carbon dioxide to form carbamates, which no longer titrate as free base. And two lots of the same nominal grade can differ in the low molecular weight tail - total amine value barely moves, but viscosity and bridging behaviour do.

The pH of a 5% solution, usually 10 to 12 at release, is a quick flag for carbon dioxide uptake. Sealed containers and a re-test before a long campaign cost less than a failed dosing trial.

6. When the PEI Grade Is Not the Problem

If the dose is calculated correctly and the result still misses, the grade itself may be wrong for the job. Charge demand depends on the pH of the stream, and a polymer chosen for one application can be the wrong molecular weight for another. Grade selection by application is a separate decision and is covered in our existing guides on how molecular weight determines PEI performance and on which grade fits water treatment, paper and adhesives.

Manufacturing & Supply Note: Alfa Chemical operates as a manufacturer of specialty chemicals with an integrated portfolio across organic chemistry, material science and life science. From our Zhengzhou, China facility we supply polyethyleneimine (PEI, CAS 9002-98-6) in five molecular weight grades - 600, 1,800, 10,000, 25,000 and 70,000 - each with a batch-specific COA that reports molecular weight by GPC, amine value by titration, and the loss on drying for that lot.

PEI Dosing: Frequently Asked Questions

Is a higher PEI amine value always better?
No. A higher value means more charge per gram, which helps neutralisation but can over-flocculate a system or raise conductivity. What matters is matching the value to the demand of your stream.
Should a PEI specification use dry basis or as-supplied?
State both, with a loss-on-drying tolerance. As-supplied figures move with water content; dry basis is the only stable way to compare two suppliers.
Does storage change the amine value on the COA?
It changes what the titration reads. Carbamate formation from carbon dioxide and moisture uptake both lower the measured value without degrading the polymer. Keep drums sealed and re-test before a long campaign.
Which figures does a PEI COA report?
Molecular weight by GPC, amine value by titration, appearance, density, pH of a 5% solution and water solubility - measured values for that lot, not reproduced specification ranges.
Evaluate the actual batch data
Review the amine value, loss on drying and pH for the grade you are considering before committing to a dosing trial.
Download batch COA
Test it in your own system
Request an analytical sample and we will include the lot certificate, so the calculation above can be run on the material you would actually receive.
Request analytical sample
Related reading
Grade selection across the 600 to 70,000 range.
How molecular weight determines PEI performance
Which grade fits water treatment, paper and adhesives.
Which PEI grade for water treatment, paper and adhesives
Specifications, packaging and COA for the product itself.
PEI product page: full specifications
📄 Cite this article
Alfa Chemical Technical Team. "Why PEI Dosage Drifts Between Batches - and How to Read the Amine Value Correctly." Alfa Chemical Technical Articles, November 2026.
URL: https://www.alfa-chemical.com/info/pei-amine-value-dosing-guide-103744924.html
Disclaimer: This article is for industrial and laboratory reference only. Not for human or animal consumption. Process parameters described here are typical starting points, not guaranteed values; actual results depend on equipment, water chemistry and batch-specific material behaviour. All product values are typical; the batch-specific Certificate of Analysis governs. Final terms are confirmed upon order and may vary by volume, destination and contract type.
You Might Also Like